You can manage bookmarks using lists, please log in to your user account for this.
Media type:
E-Article
Title:
The pyrometallurgical recovery of zinc from electric arc furnace dust (EAFD) with active carbon
Contributor:
Sinaga, G S T;
Wismogroho, A S;
Fitroturokhmah, A;
Kusumaningrum, R;
Widayatno, W B;
Hadiko, G;
Amal, M I
Published:
IOP Publishing, 2019
Published in:
IOP Conference Series: Materials Science and Engineering, 578 (2019) 1, Seite 012068
Language:
Not determined
DOI:
10.1088/1757-899x/578/1/012068
ISSN:
1757-8981;
1757-899X
Origination:
Footnote:
Description:
<jats:title>Abstract</jats:title>
<jats:p>The reduction of minor impurities (e.g., Ferrite, Magnesium, Lead, Chromium) from Zinc rich-EAFD with active carbon addition was investigated at temperature between 900-1300 °C. The result was powder with higher zinc content which then analysed by X-ray fluorescence spectroscopy (XRF), X-ray diffraction (XRD) and scanning electron microscope (SEM) equipped with X-Ray energy dispersive spectrometry (EDS). The thermogravimetry (TG) and differential thermal analysis (DTA) of EAFD and carbon mixture was conducted previously to grasp the temperature of thermic reaction of mixture. Recovery of 90wt% zinc from EAFD available was achieved up to 99.2wt% after the pyrometallurgy process at temperature 900 °C in atmosphere pressure while the extension of the time corresponds to the amount of recovered zinc dross.</jats:p>